The method describes the testing of submerged, compacted HMA in a reciprocating rolling-wheel device. This test provides information about the rate of permanent deformation from a moving, concentrated load. A laboratory compactor has been designed to prepare slab specimens. Also, the Superpave© Gyratory Compactor (SGC) has been designed to compact specimens in the laboratory. Alternatively, field cores of diameter, [150 mm (6 in.), 250 mm (10 in.), or 300 mm (12 in.)], or saw-cut slab specimens may be tested.
The test method is used to determine the premature failure susceptibility of HMA due to weakness in the aggregate structure, inadequate binder stiffness, or moisture damage. This test method measures the rut depth and number of passes to failure.
The potential for moisture damage effects are evaluated since the specimens are submerged in temperature-controlled water during loading.
All of our standards document are available in PDF (Portable Document Format), an electronic, downloadable format.You will be able to download the file in your account downloads.
After purchasing, you have the ability to assign each license to a specific user.
At any time, you are permitted to make printed copies for your and your members' reference use.