ASTM C1327-15(2019)
- Standard Test Method for Vickers Indentation Hardness of Advanced Ceramics
- standard by ASTM International, 07/01/2019
- Category: ASTM
$48.00
$24.00
1.1 This test method covers the determination of the Vickers indentation hardness of advanced ceramics. In this test, a pointed, square-based, pyramidal diamond indenter of prescribed shape is pressed into the surface of a ceramic with a predetermined force to produce a relatively small, permanent indentation. The surface projection of the two diagonals of the permanent indentation is measured using a light microscope. The average diagonal size and the applied force are used to calculate the Vickers hardness, which represents the material's resistance to penetration by the Vickers indenter. Hardness is computed as the ratio of the force to the contact surface area.

All of our standards document are available in PDF (Portable Document Format), an electronic, downloadable format.You will be able to download the file in your account downloads.

After purchasing, you have the ability to assign each license to a specific user.

At any time, you are permitted to make printed copies for your and your members' reference use.
ASTM E3050-16
Standard Specification for Denatured Ethanol for Use as Cooking and Appliance Fuel..
$21.00 $42.00
ASTM D8027-16
Standard Practice for Concentration of Select Radionuclides Using MnO2 for Measurement Purposes..
$25.00 $50.00
ASTM D4079-00(2016)
Standard Specification for Vapor-Degreasing Grade Methylene Chloride..
$21.00 $42.00