AWS D18.2:1999

  • Guide to Weld Discoloration Levels on Inside of Austenitic Stainless Steel Tube
  • standard by American Welding Society, 01/01/1999
  • Category: AWS

$64.00 $32.00

This standard addresses factors that affect weld discoloration on the inside of austenitic steel tube. The document contains a color illustration relating the discoloration to the oxygen content of the back shielding gas.
PDF

All of our standards document are available in PDF (Portable Document Format), an electronic, downloadable format.You will be able to download the file in your account downloads.

Multi-User Access

After purchasing, you have the ability to assign each license to a specific user.

Printable

At any time, you are permitted to make printed copies for your and your members' reference use.

AWS A5.24/A5.24M:2014

AWS A5.24/A5.24M:2014

Zirconium and Zirconium Alloy Welding Electrodes and Rods..

$36.00 $72.00

AWS A5.5/A5.5M:2014

AWS A5.5/A5.5M:2014

Specification for Low-Alloy Steel Electrodes for Shielded Metal Arc Welding..

$36.00 $72.00

AWS G2.4/G2.4M:2014

AWS G2.4/G2.4M:2014

Guide for the Fusion Welding of Titanium and Titanium Alloys..

$38.00 $76.00

AWS D8.1M:2013

AWS D8.1M:2013

Specification for Automotive Weld Quality - Resistance Spot Welding of Steel..

$34.00 $68.00