• NACE 61114

NACE 61114

  • Underdeposit Corrosion (UDC) Testing and Mitigation Methods in the Oil and Gas Industry
  • standard by National Association of Corrosion Engineers, 08/01/2
  • Category: NACE

$59.00 $30.00

Failures caused by UDC occurrence have been reported in the oil and gas industry in various applications. The solid deposits to be addressed in this report are limited to sand, scale, and corrosion products inside pipelines. Wax, asphaltenes, and biofilms certainly affect UDC; however, they are beyond the scope of this report. Accelerated corrosion under iron sulfide and iron carbonate films is thought to cause pitting initiation and propagation in CO2 and H2S containing environments. Pipeline mechanical cleaning becomes a key issue and is usually achieved using aggressive pigging programs on a regular basis. Moreover, corrosion inhibitors have the potential to prevent this type of corrosion, or at least minimize the pigging frequency. It is general practice to establish laboratory testing protocols that are able to assess UDC and evaluate the performance of a given inhibitor in protecting the pipe wall in the presence of solids on the surface.
PDF

All of our standards document are available in PDF (Portable Document Format), an electronic, downloadable format.You will be able to download the file in your account downloads.

Multi-User Access

After purchasing, you have the ability to assign each license to a specific user.

Printable

At any time, you are permitted to make printed copies for your and your members' reference use.

Wet H2S Cracking of Carbon Steels and Weldments
NACE 38214

NACE 38214

Manual of Biocorrosion by Hector A. Videla..

$39.00 $77.00

NACE 38219

NACE 38219

Materials for Engineering by J.W. Martin..

$24.00 $48.00

NACE RP0185-96

NACE RP0185-96

Standard Recommended Practice - Extruded Polyolefin Resin Coating Systems for Underground or Submerg..

$84.00 $167.00