• NACE SP0170-2012

NACE SP0170-2012

  • Protection of Austenitic Stainless Steels and Other Austenitic Alloys from Polythionic Acid Stress Corrosion Cracking During Shu
  • standard by National Association of Corrosion Engineers, 06/23/2
  • Category: NACE

$59.00 $30.00

This standard practice provides mitigation methods to protect austenitic stainless steels and other austenitic alloys from PTA SCC that can occur during a shutdown of refinery equipment.
For the purposes of this standard, a shutdown includes the actual downtime period and the contiguous periods required to shut down and start up the equipment.
For the purposes of this standard, the term austenitic materials includes austenitic stainless steels and other austenitic alloys.
For the purposes of this standard, the term other austenitic alloys refers to those alloys of nickel, iron, and chromium that may be susceptible to PTA SCC.
For the purposes of this standard, the term purging is defined as a flow of inert gas (in this case dry nitrogen) to free the system of impurities (oxygen).
PDF

All of our standards document are available in PDF (Portable Document Format), an electronic, downloadable format.You will be able to download the file in your account downloads.

Multi-User Access

After purchasing, you have the ability to assign each license to a specific user.

Printable

At any time, you are permitted to make printed copies for your and your members' reference use.

NACE TM0101-2001

NACE TM0101-2001

Measurement Techniques Related to Criteria for CP..

$79.00 $158.00

NACE 05101

NACE 05101

State-of-the-Art Survey on Corrosion of Steel Piling in Soils..

$30.00 $59.00

NACE TM0197-2002

NACE TM0197-2002

Laboratory Screening Test to Determine the Ability of Scale Inhibitors to Prevent the Precipitation ..

$92.00 $184.00

NACE TM0296-2002

NACE TM0296-2002

Evaluating Elastomeric Materials in Sour Liquid Environments..

$85.00 $170.00