• SAE AIR5065A

SAE AIR5065A

  • Influence of Grain Flow on Bolt Integrity (Stabilized: May 2012)
  • standard by SAE International, 05/09/2012
  • Category: SAE

$81.00 $41.00

This document has been declared "Stabilized" and will no longer be subjected to periodic reviews for currency. Users are responsible for verifying references and continued suitability or technical requirements. New technology may exist.

Performed tensile and fatigue tests on bolts to determine if cutting of materials flow lines at the bolt underhead would degrade bolt integrity. Five different alloys used in aerospace industry fatigue critical applications were employed to fabricate 5/16 to « inch diameter bolts. These bolts were machined from bar stock producing fully cut material flow lines under their heads. Tensile testing with and without underhead washers was performed along with industry standard fatigue testing.
PDF

All of our standards document are available in PDF (Portable Document Format), an electronic, downloadable format.You will be able to download the file in your account downloads.

Multi-User Access

After purchasing, you have the ability to assign each license to a specific user.

Printable

At any time, you are permitted to make printed copies for your and your members' reference use.

SAE J2881_201006

SAE J2881_201006

Measurement of Aerodynamic Performance for Mass-Produced Cars and Light-Duty Trucks..

$41.00 $81.00

SAE AS33700A

SAE AS33700A

Insert Arrangements, Electric Connector, Shell Size 12..

$41.00 $81.00

SAE AS33703A

SAE AS33703A

Insert Arrangements, Electric Connector, Shell Size 37..

$41.00 $81.00

SAE ARP5583A

SAE ARP5583A

Guide to Certification of Aircraft in a High-Intensity Radiated Field (HIRF) Environment..

$41.00 $81.00