  • Plating, Nickel-Thallium-Boron or Nickel-Boron Electroless Deposition
  • standard by SAE International, 10/03/2011
  • Category: SAE

$81.00 $41.00

This specification covers the engineering requirements for electroless deposition of a nickel-thallium-boron or nickel-boron coating on various substrates and properties of the deposit.

This process has been used typically to provide hard, ductile, wear-resistant surface for operation in service up to 1000 degrees F (538 degrees C), to provide uniform build up on complex shapes, and to enhance solderability of surfaces, but usage is not limited to such applications. This process is not generally recommended for materials subject to overtempering or high temperature embrittlement when exposed to the post-plating heat treatment of 675 \mDF (357 \mDC) for 90 minutes.
PDF

All of our standards document are available in PDF (Portable Document Format), an electronic, downloadable format.You will be able to download the file in your account downloads.

Multi-User Access

After purchasing, you have the ability to assign each license to a specific user.

Printable

At any time, you are permitted to make printed copies for your and your members' reference use.

SAE AMSR81835

SAE AMSR81835

Remover, Organic Coating, Hot Tank Type..

$41.00 $81.00

SAE AS17108A

SAE AS17108A

Bearing, Ball, Annular, Primarily for Aircraft Generators and Motor-Generators, Wide Cartridge, Type..

$41.00 $81.00

SAE AMS4940A

SAE AMS4940A

Titanium Sheet, Strip, and Plate Commercially Pure Annealed, 25.0 ksi (172 MPa) Yield Strength..

$41.00 $81.00

SAE AMS4941E

SAE AMS4941E

Titanium Tubing, Welded Annealed, 40 ksi (276 MPa) Yield Strength..

$41.00 $81.00