• SAE AMS2451/7A

SAE AMS2451/7A

  • Plating, Brush, Nickel Low Stress, Medium-Hardness Deposit
  • standard by SAE International, 04/19/2011
  • Category: SAE

$81.00 $41.00

This specification covers the engineering requirements and process for brush plating of medium-hardness, low stress nickel by electrodeposition. It should be used, in conjunction with AMS 2451, for medium-hardness, low stress nickel deposits.

This process has been used typically to provide wear resistance and to repair damaged, worn, or mismachined parts in applications requiring hardness, fatigue resistance, and service temperatures up to 450 degrees F (232 degrees C), but usage is not limited to such applications.
PDF

All of our standards document are available in PDF (Portable Document Format), an electronic, downloadable format.You will be able to download the file in your account downloads.

Multi-User Access

After purchasing, you have the ability to assign each license to a specific user.

Printable

At any time, you are permitted to make printed copies for your and your members' reference use.

SAE AMS5356C

SAE AMS5356C

Steel, Corrosion Resistant, Investment Castings 15Cr - 4.6Ni - 0.22Cb - 2.8Cu Solution and Precipita..

$41.00 $81.00

SAE AMS5581F

SAE AMS5581F

Nickel Alloy, Corrosion and Heat-Resistant, Seamless or Welded Tubing 62Ni - 21.5Cr - 9.0Mo - 3.7Cb ..

$41.00 $81.00

SAE AMS5588G

SAE AMS5588G

Nickel Alloy, Corrosion and Heat-Resistant, Welded Tubing 47.5Ni - 22Cr - 1.5Co - 9.0Mo - 0.60W - 18..

$41.00 $81.00

SAE AMS5832G

SAE AMS5832G

Nickel Alloy, Corrosion and Heat Resistant, Welding Wire, 52.5Ni - 19Cr - 3.0Mo - 5.1Cb(Nb) - 0.90Ti..

$41.00 $81.00