This method is for determining the loss on ignition of fresh or used catalysts at the specific temperature of 500 degrees C.

PDF

All of our standards document are available in PDF (Portable Document Format), an electronic, downloadable format.You will be able to download the file in your account downloads.

Multi-User Access

After purchasing, you have the ability to assign each license to a specific user.

Printable

At any time, you are permitted to make printed copies for your and your members' reference use.

UOP 379-81

UOP 379-81

Hydrogen Fluoride in HF Alkylation Regenerator Bottoms..

$120.00 $240.00

UOP 382-81

UOP 382-81

Water in Regenerator Bottoms from Hydrogen Fluoride Alkylation..

$120.00 $240.00

UOP 821-81

UOP 821-81

Automated Micro Pore Size Distribution of Porous Substances by Nitrogen Adsorption and/or Desorption..

$144.00 $287.00

UOP 437-81

UOP 437-81

Size Distribution of Molecular Sieve Particles..

$144.00 $287.00