• UOP 924-00

UOP 924-00

  • Nickel, Tungsten, Sodium and Aluminum in Hydrocracking Catalysts by ICP-AES
  • standard by UOP LLC, A Honeywell Company, 01/01/2000
  • Category: UOP

$240.00 $120.00

This method is for determining nickel(Ni), tungsten(W), sodium(Na) and aluminum(Al) in fresh alumina or alumino-silicate supported catalysts by inductively coupled plasma atomic emission spectroscopy (ICP-AES). The method is suitable for the determination of elements from the low ppm to high mass percent concentration ranges. The determination of Ni, W, Na and Al is described herein, however, many other elements which are brought into solution during the described sample decomposition can be also determined. Because of incomplete dissolution, catalysts containing alpha- or theta-alumina phases cannot be analyzed by this method, however, it can be applied if a modified sample dissolution technique, such as a TeflonTM lined pressure vessel (not described herein) is utilized.

This method can also be used for spent catalyst after suitable pretreatment.

PDF

All of our standards document are available in PDF (Portable Document Format), an electronic, downloadable format.You will be able to download the file in your account downloads.

Multi-User Access

After purchasing, you have the ability to assign each license to a specific user.

Printable

At any time, you are permitted to make printed copies for your and your members' reference use.

UOP 880-08

UOP 880-08

Hydrocarbon Types and Distributions in Low Olefin C12 and Lower Endpoint Distillates by GC..

$120.00 $240.00

UOP 551-08

UOP 551-08

C6 and Lower Boiling Hydrocarbons in Olefin Free Naphthas by GC..

$120.00 $240.00

UOP 851-08

UOP 851-08

Density of Powders and Solids by Helium Displacement..

$120.00 $240.00

UOP 373-08

UOP 373-08

Composition of C2 Through C5 Hydrocarbon Mixtures by GC..