• UOP 925-16

UOP 925-16

  • Nickel, Molybdenum, Phosphorus, Cobalt and Aluminum in Fresh Catalysts by ICP-OES
  • standard by UOP LLC, A Honeywell Company, 05/02/2016
  • Category: UOP

$240.00 $120.00

This method is for determining nickel, molybdenum, phosphorus and cobalt in fresh gamma-alumina supported catalysts; and nickel (Ni), molybdenum (Mo), phosphorus (P), cobalt (Co) and aluminum (Al) in fresh silica-alumina supported catalysts of known composition by Inductively Coupled Plasma-Optical Emission Spectrometry (ICP-OES). The method is suitable for determining nickel over a range of 1 to 10 mass-%, molybdenum over a range of 5 to 20 mass-%, phosphorus (as phosphate only) over a range of 0.5 to 25 mass-%, cobalt over a range of 1 to 5 mass-%, and aluminum over a range of 5 to 50 mass-%. Catalysts containing alpha- or theta-alumina phases cannot be analyzed by the method. Nickel bearing catalysts that also contain tungsten are analyzed by UOP Method 924.

PDF

All of our standards document are available in PDF (Portable Document Format), an electronic, downloadable format.You will be able to download the file in your account downloads.

Multi-User Access

After purchasing, you have the ability to assign each license to a specific user.

Printable

At any time, you are permitted to make printed copies for your and your members' reference use.

UOP 827-81

UOP 827-81

Apparent Hydrogen Sulfide in Amine Solutions..

$120.00 $240.00

UOP 828-81

UOP 828-81

Total Amine in Solutions..

$120.00 $240.00

UOP 379-81

UOP 379-81

Hydrogen Fluoride in HF Alkylation Regenerator Bottoms..

$120.00 $240.00

UOP 382-81

UOP 382-81

Water in Regenerator Bottoms from Hydrogen Fluoride Alkylation..

$120.00 $240.00